Bulo Mai Sauƙi Mai Nauyi na Silica yana ɗaukar ma'adinin silica da aka raba sosai a matsayin kayan da aka ƙera. Girman barbashi mai mahimmanci bai wuce 1mm ba, a ciki girman barbashi sama da 90% ƙasa da 0.5mm. Ana yin tubalin rufin silicate ta hanyar ƙara abu mai kama da wuta a cikin ɗaukar nauyi ko amfani da hanyar kumfa ta iskar gas don samar da tsari mai ramuka ta hanyar harbawa, kuma ana iya yin tubalin rufin silicate don samfurin da ba a ƙone shi ba.
Bulo Mai Sauƙi Mai Nauyin Silica yana sanya kayan aiki da ruwa a cikin kayan aiki na murƙushewa bisa ga wani rabo sannan a murƙushe shi ya zama laka, a siffanta laka zuwa tubali ta hanyar ƙera ta hanyar injina ko ma'aikata. Sannan a busar da tubalin har sai ruwan da ya rage ya yi ƙasa da 0.5%, wanda ke hana faɗaɗa girma daga canjin lu'ulu'u na SiO2 kuma a kunna tubalin da aka siffanta a cikin zafin jiki mai yawa.
| Abubuwa | QG-1.0 | QG-1.1 | QG-1.15 | QG-1.2 |
| SiO2% | ≥91 | ≥91 | ≥91 | ≥91 |
| Yawan yawa g/cm3 | ≥1.00 | ≥1.10 | ≥1.15 | ≥1.20 |
| Ƙarfin Murkushewar Sanyi MPa | ≥2.0 | ≥3.0 | ≥5.0 | ≥5.0 |
| Rashin ƙarfin juriya a ƙarƙashin kaya °C 0.1Mpa | ≥1400 | ≥1420 | ≥1500 | ≥1520 |
| Sake Dumamawa Canjin Layi (%) 1450°C×2h | 0~+0.5 | 0~+0.5 | 0~+0.5 | 0~+0.5 |
| Faɗaɗa Ma'aunin Zafi na 20-1000°C ×10-6℃-1 | 1.3 | 1.3 | 1.3 | 1.3 |
| Matsakaicin Da'irar Zafi (W/(m·K) 350°C±10℃ | ≤0.55 | ≤0.6 | ≤0.65 | ≤0.7 |
Ana iya amfani da tubalin da ke hana ruwa shiga cikin siliki a cikin tanderun gilashi da murhun zafi, kuma ana iya amfani da tubalin hana ruwa shiga cikin siliki a cikin tanda na coke, tanderun carbon da duk wani tanderun masana'antu.